{"product_id":"progress-on-pellet-cladding-interaction-and-stress-corrosion-cracking-experimentation-modelling-and-methodologies-applied-to-support-the-flexible-operation-of-nuclear-power-plants-report-of-a-technical-meeting-9789201165213","title":"Progress on Pellet–Cladding Interaction and","description":"\u003cb\u003eBook Synopsis\u003c\/b\u003e\u003cbr\u003eFlexible operation and related power changes can have a direct impact on fuel integrity through pellet–cladding interaction\/stress corrosion cracking (PCI\/SCC) phenomena, which could lead to fuel failures in certain conditions. For some anticipated operational occurrences that affect fuel with small PCI\/SCC margins, the fuel failures caused by PCI\/SCC cannot be assumed to be benign, and a significant radiological source term may be generated. This publication provides an overview of PCI\/SCC studies and reports on the progress made since the early 2000s, based on presentations and discussions at a related IAEA technical meeting held in October 2019.","brand":"IAEA","offers":[{"title":"Default Title","offer_id":50473185247575,"sku":"9789201165213","price":15.15,"currency_code":"GBP","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0817\/1739\/5799\/files\/9789201165213.jpg?v=1744905633","url":"https:\/\/bookcurl.com\/products\/progress-on-pellet-cladding-interaction-and-stress-corrosion-cracking-experimentation-modelling-and-methodologies-applied-to-support-the-flexible-operation-of-nuclear-power-plants-report-of-a-technical-meeting-9789201165213","provider":"Book Curl","version":"1.0","type":"link"}